We make safety even safer.

Upon completion of the production process and at customers' request, our safety glass runs through the Heat-Soak-Test in accordance with EN 14179. With this testing method almost every glass that tends to spontaneous disintegration due to nickel sulphide inclusions can be sorted out. Only glass panes with a positive test result leave our plant.

Our online-aided heat-soak-oven of the latest generation tests safety glass units for their stress equilibrium, thus allowing the processing of dimensions up to 6.0 m x 2.6 m. Both the oven and the measuring procedure have been checked and certified by an independent institute. The certified production of coated TSG-H glass is also ensured with immediate effect. 